Fractographic and Microstructural Analysis of Fatigue Specimens of A302 Grade B Steel Tested in Air at Room Temperature
Author | : G. Gabetta |
Publisher | : |
Total Pages | : 26 |
Release | : 1979 |
ISBN-10 | : UOM:39015095232867 |
ISBN-13 | : |
Rating | : 4/5 ( Downloads) |
Download or read book Fractographic and Microstructural Analysis of Fatigue Specimens of A302 Grade B Steel Tested in Air at Room Temperature written by G. Gabetta and published by . This book was released on 1979 with total page 26 pages. Available in PDF, EPUB and Kindle. Book excerpt: